| Item | Specification |
|---|---|
| Alloy Or Not | Alloy |
| Material | Nickel Based Cast Superalloy |
| Grade | K405 |
| China ISC No. | C74050 |
| Old Grade | K5 |
| Equivalent Grade | K405 / K5 |
| Shape | Casting / Cast Components |
| Processing Service | Precision Casting / Machining |
| Nickel Content | Remainder |
| Chromium Content | 9.5–11 |
| Molybdenum Content | 3.5–4.2 |
| Tungsten Content | 4.5–5.2 |
| Cobalt Content | 9.5–10.5 |
| Aluminum Content | 5–5.8 |
| Titanium Content | 2–2.9 |
| Elongation | ≥ 5 |
| Place of Origin | Zhejiang, China |
| Brand Name | Shuaiyi |
| Size | As your requirement |
| MOQ | 200 kg / Flexible |
| Standard | GB/T 14992-2025 |
| Package | Standard Seaworthy Package |
| Sample | Available |
| Element | Content (%) |
|---|---|
| C | 0.11–0.18 |
| Si | ≤ 0.3 |
| Mn | ≤ 0.5 |
| P | ≤ 0.02 |
| S | ≤ 0.01 |
| Cr | 9.5–11 |
| Ni | Remainder |
| Mo | 3.5–4.2 |
| W | 4.5–5.2 |
| Co | 9.5–10.5 |
| B | 0.015–0.026 |
| Al | 5–5.8 |
| Ti | 2–2.9 |
| Fe | ≤ 0.5 |
| Zr | 0.05–0.1 |
| Ce | ≤ 0.01 |









We supply stainless steel, high-temperature alloy, special steel, copper and aluminum alloy. Available product forms include plates, tubes, rods, strips, forgings, flanges and welding materials for nuclear power, chemical, aerospace, marine and automotive industries.
Yes. All products comply with ASTM, ASME, DIN and JIS standards. We own SGS, TUV authoritative certification, with complete UT, hydraulic test and spectrometer testing equipment for strict full quality inspection.
Yes. We support custom cutting, bending, forging and shaping with advanced laser, waterjet and plasma cutting technology. One-stop manufacturing meets personalized technical requirements.
We have sufficient in-stock reserves with a monthly warehouse stock of 2000 tons and stable port throughput. Equipped with advanced professional production equipment, we support fast bulk order production and timely global delivery.
Free metal samples are available. We provide one-stop procurement solutions and professional technical after-sales service to solve all material application problems for global clients.
TC21 is a high-strength and damage-tolerance alpha-beta titanium alloy. Its nominal composition is Ti-6Al-2Sn-2Zr-3Mo-1Cr-2Nb with silicon as a minor alloying element. It is designed for applications requiring a combination of strength, fracture toughness and damage tolerance.
TC17 is a high-strength alpha-beta titanium alloy with nominal composition Ti-5Al-2Sn-2Zr-4Mo-4Cr. Its microstructure and heat-treatment response allow it to achieve a high strength level while maintaining useful ductility, making it suitable for demanding aerospace structural and engine applications.
TC11 is a heat-resistant alpha-beta titanium alloy with nominal composition Ti-6.5Al-3.5Mo-1.5Zr-0.3Si. It offers good high-temperature strength and hot-working performance and is widely associated with compressor components such as blades, discs, drums and shafts.
TC6 is an alpha-beta titanium alloy with a combination of strength, thermal performance and hot-workability. Its nominal composition is Ti-6Al-2.5Mo-1.5Cr-0.5Fe-0.3Si, and it is used particularly for high-strength aerospace engine components.
TC4 is the Chinese designation for Ti-6Al-4V and corresponds to ASTM Grade 5. It is one of the most widely used alpha-beta titanium alloys, offering high specific strength, good corrosion resistance, good fatigue performance and versatile processing characteristics.
TC1 is a low-alloy alpha-beta titanium alloy based on the Ti-Al-Mn system. It provides a combination of moderate strength, good formability, weldability and corrosion resistance and can be processed into plates, sheets and other semi-finished products.